Fully compliant with SPLN 41-8 standards for Aluminum Alloy Conductors (AAAC).
The outermost layer is precision-twisted to the right (Z-direction) for optimal structural integrity.
| Aluminum Alloy Conductor (AAAC) Technical Data | |||||||
|---|---|---|---|---|---|---|---|
| Code Name | Sectional Area | Wire Diameter & Stranding | Diameter of Conductor | Nominal Breaking Load | Linear Mass | Maximum Resistance at 20℃ | |
| mm² | mm | No. | mm | N | kg/km | Ω/km | |
| 16 | 16.8 | 1.75 | 7 | 5.25 | 4704 | 46.1 | 1.955 |
| 25 | 27.8 | 2.25 | 7 | 6.75 | 7742 | 76.2 | 1.183 |
| 35 | 34.4 | 2.5 | 7 | 7.5 | 9604 | 94.1 | 0.958 |
| 50 | 49.5 | 3.00 | 7 | 9 | 13818 | 135.5 | 0.665 |
| 45.7 | 1.75 | 19 | 8.75 | 12740 | 125.8 | 0.724 | |
| 55 | 58.1 | 3.25 | 7 | 9.75 | 16219 | 159.0 | 0.567 |
| 70 | 75.5 | 2.25 | 19 | 11.25 | 21070 | 207.9 | 0.438 |
| 95 | 93.3 | 2.50 | 19 | 12.5 | 26068 | 256.6 | 0.355 |
| 100 | 99.3 | 4.25 | 7 | 12.75 | 27734 | 271.9 | 0.332 |
| 120 | 112.9 | 2.75 | 19 | 13.75 | 31556 | 310.5 | 0.293 |
| 150 | 157.6 | 3.25 | 19 | 16.25 | 44002 | 433.7 | 0.210 |
| 147.1 | 2.25 | 37 | 15.75 | 41062 | 405.8 | 0.225 | |
| 185 | 181.6 | 2.5 | 37 | 17.5 | 50715 | 500.9 | 0.183 |
| 240 | 238.8 | 4 | 19 | 20 | 66689 | 657.0 | 0.137 |
| 242.5 | 2.25 | 61 | 20.25 | 67718 | 670.3 | 0.139 | |
| 300 | 299.4 | 2.5 | 61 | 22.5 | 83594 | 827.5 | 0.1110 |
| 400 | 431.2 | 3.00 | 61 | 27 | 120442 | 1191.6 | 0.077 |
| 500 | 506.0 | 3.25 | 61 | 29.25 | 141316 | 1398.5 | 0.066 |
| 630 | 643.2 | 3 | 91 | 33 | 179634 | 1784.9 | 0.052 |
| 800 | 754.9 | 3.25 | 91 | 35.75 | 210847 | 2094.8 | 0.044 |
| 1000 | 1005.1 | 3.75 | 91 | 41.25 | 280672 | 2789.0 | 0.033 |